10 COMMENTS

  1. Hello Everyone, I have a problem with anodising the pressure casting aluminium, means the alloy with high silicon contain (Si>6%). Does anybody tried this? Which parameter could be a problem, which should be combined?

  2. clear anodizing very easy…hahahaha
    try black colour..why no rinse after sealing..if u anodize black colour with sand blasting surface u can see the sealing mark at surface..btw..better use rinse after sealing for adviod dirty from chemical